Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Platinum, platinum alloy

Characteristics for grade     PlPdRe900-80   ( ПлПдРе900-80 )



      Grade :     PlPdRe900-80   ( ПлПдРе900-80 )
      Classification :   Platinum for jewellery
      Equivalent grades:     Is absent



Chemical composition in % for grade   PlPdRe900-80   ( ПлПдРе900-80 )
Fe Si PbY AuPtPdReImpurity
max   0.04max   0.009max   0.0150.01 - 0.1max   0.0590 - 90.57.5 - 8.50.67 - 2.38 all 0.11
Comment: Re is a basis; the percentage of Re is given approximately.


Technological properties of the material   PlPdRe900-80   ( ПлПдРе900-80 ) .
        Melting temperature : 1680 - 1740   °C


Physical properties for grade   PlPdRe900-80   ( ПлПдРе900-80 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       20200    



Types of delivery of grade   PlPdRe900-80   ( ПлПдРе900-80 )
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  PlPdRe900-80   ( ПлПдРе900-80 ) - Platinum for jewellery: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru