Characteristics for grade     60S2KHА   ( 60С2ХА )

      Grade :     60S2KHА   ( 60С2ХА )
      Substitute:   60С2ХФА, 60С2Н2А
      Classification :   Spring structural steel
      Equivalent grades:   Go here



Chemical composition in % for grade   60S2KHА   ( 60С2ХА )
C Si Mn Ni S P Cr Cu
0.56 - 0.641.4 - 1.80.4 - 0.7max   0.25max   0.025max   0.0250.7 - 1max   0.2


Temperature of critical points for grade   60S2KHА   ( 60С2ХА ).
Ac1 = 765 ,      Ac3(Acm) = 780 ,       Ar1 = 700


Mechanical properties under Т=20oС for grade   60S2KHА   ( 60С2ХА )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Steel, GOST 14959-79     1470 1325 6 25 Guenching 870oC, oil, Drawing 470oC,


    Brinell hardness for     60S2KHА   ( 60С2ХА )   (without heat treatment) ,       GOST 14959-79 HB 10 -1 = 321   MPa
    Brinell hardness for     60S2KHА   ( 60С2ХА )   (heat treatment) ,     Rolled stock GOST 14959-79 HB 10 -1 = 285   MPa


Technological properties for grade   60S2KHА   ( 60С2ХА )
  Weldability: is not used.
 Flakes : not predisposed
Temper brittleness: not predisposed


Physical properties for grade   60S2KHА   ( 60С2ХА )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.96          


Equivalent steels for grade     60S2KHА   ( 60С2ХА )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyChinaSwedenBulgariaPolandRomaniaCzechia
-DIN,WNrJIS AFNORBSEN UNIGBSSBDSPNSTASCSN
9254
9260
G92540
1.7102
1.7103
54SiCr6
60SiCr7
67SiCr5
SUP12
SUP7
54SiCr6
60SC7
61SC7
250A61
685H57
1.7102
54SiCr6
48Si7
60SiCr8
60Si2CrA
2090
60S2A
60S2ChA
60S2
60S2A
60Si15A
13270
14260

Types of delivery of grade   60S2KHА   ( 60С2ХА )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В72 - Medium-high and high-carbon steel wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  60S2KHА   ( 60С2ХА ) - Spring structural steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru