Characteristics for grade     65S2VА   ( 65С2ВА )

      Grade :   65S2VА   ( 65С2ВА ) (   65С2ГВА   )
      Substitute:   60С2А, 60С2ХА
      Classification :   Spring structural steel
      Equivalent grades:   Go here
Grade   65S2VА   ( 65С2ВА ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   65S2VА   ( 65С2ВА )
C Si Mn Ni S P Cr W Cu
0.61 - 0.691.5 - 20.7 - 1max   0.25max   0.025max   0.025max   0.30.8 - 1.2max   0.2


Mechanical properties under Т=20oС for grade   65S2VА   ( 65С2ВА )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Band annealed , GOST 2283-79 0.1 - 4   880   8    
Band cold-worked , GOST 2283-79 0.1 - 4   780-1180       
Steel, GOST 14959-79     1860 1665 5 20 Guenching 850oC, oil, Drawing 420oC,


    Brinell hardness for     65S2VА   ( 65С2ВА )   (without heat treatment) ,       GOST 14959-79 HB 10 -1 = 321   MPa
    Brinell hardness for     65S2VА   ( 65С2ВА )   (heat treatment) ,     Rolled stock GOST 14959-79 HB 10 -1 = 285   MPa


Technological properties for grade   65S2VА   ( 65С2ВА )
  Weldability: is not used.
 Flakes : not predisposed
Temper brittleness: not predisposed


Physical properties for grade   65S2VА   ( 65С2ВА )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.11   27 7850    
100 2.06 11.5 27   475  
200 2 12.5 28   500  
300 1.95 13 29   510  
400 1.85 13.5 29   530  
500 1.78 13.8 29   555  
600 1.54 14.3 29   580  
700 1.36 14.5 28   615  
800 1.31 13.5 28   690  
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     65S2VА   ( 65С2ВА )
Warning! Indicated both exact and nearest equivalents.
FranceBulgariaPolandRomania
AFNORBDSPNSTAS
45SCD6
65S2VA
65S2WA
652SW

Types of delivery of grade   65S2VА   ( 65С2ВА )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В72 - Medium-high and high-carbon steel wire
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  65S2VА   ( 65С2ВА ) - Spring structural steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru