Characteristics for grade     KH12MF   ( Х12МФ )

      Grade :     KH12MF   ( Х12МФ )
      Substitute:   Х6ВФ, Х12Ф1, Х12ВМ
      Classification :   Die tool steel
      Equivalent grades:   Go here
Grade   KH12MF   ( Х12МФ ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 376-298-00 ,     info [a] auremo.org



Chemical composition in % for grade   KH12MF   ( Х12МФ )
C Si Mn Ni S P Cr Mo V Cu
1.45 - 1.650.1 - 0.40.15 - 0.45max   0.4max   0.03max   0.0311 - 12.50.4 - 0.60.15 - 0.3max   0.3


Temperature of critical points for grade   KH12MF   ( Х12МФ ).
Ac1 = 810 ,      Ac3(Acm) = 860 ,       Ar3(Arcm) = 780 ,       Ar1 = 760 ,       Mn = 225


    Brinell hardness for     KH12MF   ( Х12МФ )   (annealing) ,       GOST 5950-2000 HB 10 -1 = 255   MPa


Technological properties for grade   KH12MF   ( Х12МФ )
  Weldability: is not used.
Temper brittleness: predisposed


Equivalent steels for grade     KH12MF   ( Х12МФ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainSwedenBulgariaHungaryPolandCzechiaAustria
-DIN,WNrJIS AFNORBSEN UNIUNESSBDSMSZPNCSNONORM
D2
T30402
1.2379
1.2601
X162CrMoV12
X165CrMoV12
Х155CrVMo12-1
SKD11
X160CrMoV12
Z160CDV12
BD2
X160CrMoV12-1
C165CrMoV12KU
X155CrVMo12-1KU
X160CrMoV12
2310
Ch12MF
K8
NC11LV
19572
K105

Types of delivery of grade   KH12MF   ( Х12МФ )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  KH12MF   ( Х12МФ ) - Die tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru