Grade : | 7KHG2VMF ( 7ХГ2ВМФ ) |
Classification : | Die tool steel |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Mo | W | V | Cu |
0.68 - 0.76 | 0.1 - 0.4 | 1.8 - 2.3 | max 0.4 | max 0.03 | max 0.03 | 1.5 - 1.8 | 0.5 - 0.8 | 0.55 - 0.9 | 0.1 - 0.25 | max 0.3 |
Ac1 = 765 , Ac3(Acm) = 825 , Ar3(Arcm) = 430 , Ar1 = 310 , Mn = 160 |
Brinell hardness for 7KHG2VMF ( 7ХГ2ВМФ ) (annealing) , GOST 5950-2000 | HB 10 -1 = 255 MPa |
USA | |
- | |
|
В32 - Graded and shaped rolling |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |