Characteristics for grade     in000   ( Ин000 )



      Grade :     in000   ( Ин000 )
      Classification :   Indium
      Equivalent grades:     Is absent



Chemical composition in % for grade   in000   ( Ин000 )
FeMn Ni SAl Cu As Pb Se Mg Zn Ag Bi Sn Te CdGaInImpurity
max   0.00002max   0.000001max   0.00002max   0.00005max   0.00003max   0.000008max   0.00005max   0.00002max   0.00005max   0.00003max   0.00002max   0.000001max   0.00003max   0.00005max   0.00001max   0.000003max   0.00008min   99.9995 all 0.0005



Types of delivery of grade   in000   ( Ин000 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  in000   ( Ин000 ) - Indium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru