Characteristics for grade     in00   ( Ин00 )



      Grade :     in00   ( Ин00 )
      Classification :   Indium
      Equivalent grades:     Is absent



Chemical composition in % for grade   in00   ( Ин00 )
Fe NiAl Cu As Pb Mg Zn Ag Sn CdTlInImpurity
max   0.00005max   0.00002max   0.0001max   0.00001max   0.00005max   0.0001max   0.00003max   0.0001max   0.0001max   0.0001max   0.00001max   0.0001min   99.999 all 0.001



Types of delivery of grade   in00   ( Ин00 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  in00   ( Ин00 ) - Indium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys