Grade : | 4KHMFS ( 4ХМФС ) ( 40ХСМФ ) |
Classification : | Die tool steel |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Mo | V | Cu |
0.37 - 0.45 | 0.5 - 0.8 | 0.5 - 0.8 | max 0.4 | max 0.03 | max 0.03 | 1.5 - 1.8 | 0.9 - 1.2 | 0.3 - 0.5 | max 0.3 |
Ac1 = 760 , Ac3(Acm) = 805 , Ar3(Arcm) = 710 , Ar1 = 630 , Mn = 280 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Die | to 500 | 1450 | 1280 | 7 | 20 | 200 | Guenching 950oC, oil, Drawing 550oC, |
Brinell hardness for 4KHMFS ( 4ХМФС ) (heat treatment) , GOST 5950-2000 | HB 10 -1 = 241 MPa |
Germany | France | Austria | |||
DIN,WNr | AFNOR | ONORM | |||
|
|
|
В22 - Graded and shaped rolling |
B31 - Blanks, Blanks, Slabs |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |