Characteristics for grade     Rd99.8   ( Рд99.8 )



      Grade :     Rd99.8   ( Рд99.8 )
      Classification :   Rhodium
      Equivalent grades:     Is absent



Chemical composition in % for grade   Rd99.8   ( Рд99.8 )
Fe Si Ba PbAuRhImpurity -
max   0.02max   0.03max   0.008max   0.01max   0.01min   99.8 all 0.2 Pt+Pd+Ir+Ru =< 0.15


Mechanical properties under Т=20oС for grade   Rd99.8   ( Рд99.8 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire, GOST 13098-2006     600-1000       


    Brinell hardness for     Rd99.8   ( Рд99.8 )   ,     Wire GOST 13098-2006 HB 10 -1 = 110 - 140   MPa


Technological properties of the material   Rd99.8   ( Рд99.8 ) .
        Melting temperature : 1966   °C


Physical properties for grade   Rd99.8   ( Рд99.8 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       12450   500



Types of delivery of grade   Rd99.8   ( Рд99.8 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  Rd99.8   ( Рд99.8 ) - Rhodium: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru