Characteristics for grade     3KH3M3F   ( 3Х3М3Ф )



      Grade :     3KH3M3F   ( 3Х3М3Ф )
      Classification :   Die tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   3KH3M3F   ( 3Х3М3Ф )
C Si Mn Ni S P Cr Mo V Cu
0.27 - 0.340.1 - 0.40.2 - 0.5max   0.4max   0.03max   0.032.8 - 3.52.5 - 30.4 - 0.6max   0.3


Temperature of critical points for grade   3KH3M3F   ( 3Х3М3Ф ).
Ac1 = 815 ,      Ac3(Acm) = 875 ,       Ar3(Arcm) = 820 ,       Ar1 = 760 ,       Mn = 340


Mechanical properties under Т=20oС for grade   3KH3M3F   ( 3Х3М3Ф )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Steel     1670 1470   50220Guenching 1040oC, oil, Drawing 600oC, 2h,


    Brinell hardness for     3KH3M3F   ( 3Х3М3Ф )   (heat treatment) ,       GOST 5950-2000 HB 10 -1 = 229   MPa


Physical properties for grade   3KH3M3F   ( 3Х3М3Ф )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.07   32 7828   314
100     34 7808   365
200     36 7783   430
300 1.77   36 7754   515
400     36 7721   600
500     36 7684   710
600     34 7642   835
700     34 7597   965
800     33 7565   1118
900     34 7525   1151
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     3KH3M3F   ( 3Х3М3Ф )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainBulgariaHungaryPolandRomaniaCzechiaAustria
-DIN,WNrJIS AFNORBSEN UNIUNEBDSMSZPNSTASCSNONORM
H10
H12
T20810
1.2365
30CrMoV12
45WCrV7
X30WCrV5-3
X30WCrV9-3
X32CrMoV3-3
X32CrMoV33
SKD62
SKD7
32CDV12-28
32CrMoV12-28
Z35CWDV5
2365
BH10
BH12
1.2365
1.6580
30CrMoV12-11
30CrNiMo8
32CrMoV12-28
30CrMoV12-27KU
30CrMoV12
32CrMoV12-28
CMV40
K14
WLV
31VMoCr29
19541
BOHLERW320
W320



Types of delivery of grade   3KH3M3F   ( 3Х3М3Ф )
В22 - Graded and shaped rolling
B31 - Blanks, Blanks, Slabs
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  3KH3M3F   ( 3Х3М3Ф ) - Die tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru