Characteristics for grade     5KHV2S   ( 5ХВ2С )

      Grade :     5KHV2S   ( 5ХВ2С )
      Substitute:   6ХВ2С
      Classification :   Die tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   5KHV2S   ( 5ХВ2С )
C Si Mn Ni S P Cr Mo W V Cu
0.45 - 0.550.8 - 1.10.15 - 0.45max   0.35max   0.03max   0.030.9 - 1.2max   0.31.8 - 2.3max   0.3max   0.3


Temperature of critical points for grade   5KHV2S   ( 5ХВ2С ).
Ac1 = 775 ,      Ac3(Acm) = 860 ,       Mn = 295


Mechanical properties under Т=20oС for grade   5KHV2S   ( 5ХВ2С )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Steel     1470 1290 10 30230Guenching 880oC, oil, Drawing 500oC, 2h,


    Brinell hardness for     5KHV2S   ( 5ХВ2С )   (annealing) ,       HB 10 -1 = 229 - 255   MPa


Technological properties for grade   5KHV2S   ( 5ХВ2С )
  Weldability: is not used.
 Flakes : predisposed
Temper brittleness: weakly predisposed


Physical properties for grade   5KHV2S   ( 5ХВ2С )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20           300
100         462  
200           420
300         462  
400            
500           690
600         655  
700            
800           1080
900         832 1150
1000         752  
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     5KHV2S   ( 5ХВ2С )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFranceEnglandEuropeanItalySpainPolandCzechiaAustria
-DIN,WNrAFNORBSEN UNIUNEPNCSNONORM
S1
S2
SI
1.2542
45WCrV7
60WCrV
55WC20
BS1
1.2550
55WCrV8
60WCrV8
55WCrV8KU
45WCrSi8
NZ3
19733
K455

Types of delivery of grade   5KHV2S   ( 5ХВ2С )
В22 - Graded and shaped rolling
B31 - Blanks, Blanks, Slabs
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  5KHV2S   ( 5ХВ2С ) - Die tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru