Characteristics for grade     R9   ( Р9 )



      Grade :     R9   ( Р9 )
      Substitute:   Р18
      Classification :   High speed tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   R9   ( Р9 )
C Si Mn Ni S P Cr Mo W V Co
0.85 - 0.95max   0.5max   0.5max   0.4max   0.03max   0.033.8 - 4.4max   18.5 - 9.52.3 - 2.7max   0.5


Temperature of critical points for grade   R9   ( Р9 ).
Ac1 = 820 ,      Ac3(Acm) = 870 ,       Ar3(Arcm) = 780 ,       Ar1 = 740 ,       Mn = 180


Mechanical properties under Т=20oС for grade   R9   ( Р9 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
      840 490 10 29260As-delivered state
Band annealed , GOST 2283-79 0.1 - 4   880        


    Brinell hardness for     R9   ( Р9 )   (annealing) ,       HB 10 -1 = 255   MPa


Physical properties for grade   R9   ( Р9 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.2     8300   380
100     23     417
200     25     505
300     26     600
400     28     695
500     30     790
600     31     900
700           1020
800           1160
900           1170
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     R9   ( Р9 )
Warning! Indicated both exact and nearest equivalents.
Czechia
CSN
422992



Types of delivery of grade   R9   ( Р9 )
B34 - Ribbons


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  R9   ( Р9 ) - High speed tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru