Characteristics for grade     PA-ZhGrDMs   ( ПА-ЖГрДМс )



      Grade :     PA-ZhGrDMs   ( ПА-ЖГрДМс )
      Classification :   Iron-based powder antifriction materials
      Equivalent grades:     Is absent



Chemical composition in % for grade   PA-ZhGrDMs   ( ПА-ЖГрДМс )
C Ni S Mo Cu -
0.6 - 1.3max   1.51.5 - 2.41.5 - 3.62.5 - 3.5 Fe - basis


Mechanical properties under Т=20oС for grade   PA-ZhGrDMs   ( ПА-ЖГрДМс )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 26802-86     200      40 



Types of delivery of grade   PA-ZhGrDMs   ( ПА-ЖГрДМс )
В56 - Hard alloys, metal-ceramic products and metal powders


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  PA-ZhGrDMs   ( ПА-ЖГрДМс ) - Iron-based powder antifriction materials: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru