Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | R9M4K8 ( Р9М4К8 ) |
Classification : | High speed tool steel |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | Mo | W | V | Co | Cu |
1 - 1.1 | 0.2 - 0.5 | 0.2 - 0.5 | max 0.6 | max 0.03 | max 0.03 | 3 - 3.6 | 3.8 - 4.3 | 8.5 - 9.5 | 2.3 - 2.7 | 7.5 - 8.5 | max 0.25 |
Ac1 = 800 , Ac3(Acm) = 840 , Ar3(Arcm) = 790 , Ar1 = 750 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
960 | 540 | 7 | 10 | 80 | As-delivered state |
Brinell hardness for R9M4K8 ( Р9М4К8 ) (annealing) , GOST 19265-73 | HB 10 -1 = 285 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 2.29 | 8300 | ||||
100 | 25 | |||||
200 | 27 | |||||
300 | 28 | |||||
400 | 29 | |||||
500 | 30 | |||||
600 | 31 | |||||
700 | 32 | |||||
800 | ||||||
900 | 32 | |||||
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
USA | Germany | Japan | France | England | Italy | Sweden | Bulgaria | Hungary | Poland | ||||||||||
- | DIN,WNr | JIS | AFNOR | BS | UNI | SS | BDS | MSZ | PN | ||||||||||
|
|
|
|
|
|
|
|
|
|
В22 - Graded and shaped rolling |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |