Characteristics for grade     EhP975-ID   ( ЭП975-ИД )

      Grade :   EhP975-ID   ( ЭП975-ИД ) (   ЭП975ИД     ЖС6УД   )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   EhP975-ID   ( ЭП975-ИД )
Fe C Si Mn Ni S P Cr Ce Mo W Co Nb TiAl Zr BImpurity -
max   10.1 - 0.16max   0.4max   0.449.11 - 58.5max   0.01max   0.0157.5 - 9max   0.030.8 - 1.59.5 - 1114.1 - 171 - 22 - 2.74.5 - 5.1max   0.04max   0.035 all 0.5 Ni - basis


Mechanical properties under Т=20oС for grade   EhP975-ID   ( ЭП975-ИД )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
      1250 950 14 16400 


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  EhP975-ID   ( ЭП975-ИД ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru