Characteristics for grade     M-MP   ( М-МП )



      Grade :     M-MP   ( М-МП )
      Classification :   Powder material on the basis of molybdenum
      Equivalent grades:     Is absent



Chemical composition in % for grade   M-MP   ( М-МП )
Fe Si Ni WAl Ca Mg ONa -
max   0.014max   0.005max   0.005max   0.4max   0.005max   0.007max   0.003max   0.3max   0.015 K =< 0.05, Mo - basis


Mechanical properties under Т=20oС for grade   M-MP   ( М-МП )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 17431-72     640-690  8-10   
Bar, GOST 17432-72     590-640  15-20   



Types of delivery of grade   M-MP   ( М-МП )
B53 - Sheets and Strips
B55 - Bars


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  M-MP   ( М-МП ) - Powder material on the basis of molybdenum: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru