Characteristics for grade     06Kh16N15M3B   ( 06Х16Н15М3Б )

      Grade :   06Kh16N15M3B   ( 06Х16Н15М3Б ) (   06Х16Н15М3Б-ИД     ЭИ847-ИД   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   06Kh16N15M3B   ( 06Х16Н15М3Б )
C Si Mn Ni S P Cr Mo Nb
0.04 - 0.06max   0.30.4 - 0.815 - 16max   0.01max   0.01515 - 162.7 - 3.2max   0.9


Mechanical properties under Т=20oС for grade   06Kh16N15M3B   ( 06Х16Н15М3Б )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe     539   35    


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  06Kh16N15M3B   ( 06Х16Н15М3Б ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru