Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | 12GF-Sh ( 12ГФ-Ш ) ( 12ГФ ) |
Classification : | Structural steel for welding construct |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | V | Al | Cu |
0.09 - 0.14 | 0.17 - 0.37 | 0.7 - 1 | max 0.3 | max 0.012 | max 0.02 | max 0.3 | 0.04 - 0.08 | 0.02 - 0.06 | max 0.4 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe | 415-570 | 240-290 | 22-24 |
Brinell hardness for 12GF-Sh ( 12ГФ-Ш ) , Pipe | HB 10 -1 = 200 MPa |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2018 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. Previous address of this website was splav.kharkov.com |