Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     KhN33BS   ( ХН33БС )

      Grade :     KhN33BS   ( ХН33БС )
      Classification :   Hidh-temperature or heat-resistant alloy
      Equivalent grades:     Is absent
Grade   KhN33BS   ( ХН33БС ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   KhN33BS   ( ХН33БС )
C Si Mn Ni S P Cr Ce Mo W V Co Nb TiAl Cu As PbZn Sn -
0.3 - 0.40.45 - 0.950.8 - 1.4530 - 33max   0.02max   0.02520 - 230.07 - 0.11max   0.250.05 - 0.20.0005 - 0.15max   0.11 - 1.70.0005 - 0.150.0005 - 0.1max   0.2max   0.01max   0.01max   0.01max   0.01 Fe - basis


Mechanical properties under Т=20oС for grade   KhN33BS   ( ХН33БС )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe     490 245 8    


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  KhN33BS   ( ХН33БС ) - Hidh-temperature or heat-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru