Characteristics for grade     75KHMF   ( 75ХМФ )



      Grade :     75KHMF   ( 75ХМФ )
      Substitute:   75ХМ, 9ХФ
      Classification :   Tool steel for roller
      Equivalent grades:     Is absent



Chemical composition in % for grade   75KHMF   ( 75ХМФ )
C Si Mn Ni S P Cr Mo V
0.7 - 0.80.2 - 0.60.2 - 0.7max   0.3max   0.04max   0.041.4 - 1.70.1 - 0.30.05 - 0.25


Temperature of critical points for grade   75KHMF   ( 75ХМФ ).
Ac1 = 760 - 790


    Brinell hardness for     75KHMF   ( 75ХМФ )   (normalize, tempering) ,       HB 10 -1 = 241 - 285   MPa
    Brinell hardness for     75KHMF   ( 75ХМФ )   (quenching, tempering) ,       HB 10 -1 = 352 - 429   MPa


Technological properties for grade   75KHMF   ( 75ХМФ )
  Weldability: hard weldability.
 Flakes : weakly predisposed




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  75KHMF   ( 75ХМФ ) - Tool steel for roller: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys