Characteristics for grade     08KH17T   ( 08Х17Т )

      Grade :   08KH17T   ( 08Х17Т ) (   0Х17Т     ЭИ645   )
      Substitute:   12Х17, 08Х18Т1
      Classification :   Corrosion-resistant high-temperature steel
      Equivalent grades:   Go here
Grade   08KH17T   ( 08Х17Т ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 376-298-00 ,     info [a] auremo.org



Chemical composition in % for grade   08KH17T   ( 08Х17Т )
C Si Mn Ni S P Cr Ti Cu
max   0.08max   0.8max   0.8max   0.6max   0.025max   0.03516 - 18max   0.8max   0.3


Mechanical properties under Т=20oС for grade   08KH17T   ( 08Х17Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     372   17    
Pipe hot strain, GOST 9940-81     372   17    
Sheet trick, GOST 7350-77     440   18   Annealing
Sheet thin, GOST 5582-75     460   20   Annealing 740 - 780oC,


Technological properties for grade   08KH17T   ( 08Х17Т )
  Weldability: limited weldability.
Temper brittleness: predisposed


Physical properties for grade   08KH17T   ( 08Х17Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.06   25 7700   600
100   10     462  
200   10        
300   10.5        
400   10.5        
500   11        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     08KH17T   ( 08Х17Т )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEuropeanItalySpainPolandCzechia
-DIN,WNrJIS AFNOREN UNIUNEPNCSN
430Ti
439
S43036
S43900
TP430Ti
1.4510
X3CrTi17
X6CrTi17
X8CrNb17
X8CrTi17
SUS430LX
Z4CT17
Z8CT17
1.4510
X3CrTi17
X5CrTi17
X3CrTi17
X6CrTi17
F.3115
X5CrTi17
0H17T
17041

Types of delivery of grade   08KH17T   ( 08Х17Т )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  08KH17T   ( 08Х17Т ) - Corrosion-resistant high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru