Characteristics for grade     95KH18   ( 95Х18 )

      Grade :   95KH18   ( 95Х18 ) (   9Х18     ЭИ229   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here
Grade   95KH18   ( 95Х18 ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 376-298-00 ,     info [a] auremo.org



Chemical composition in % for grade   95KH18   ( 95Х18 )
C Si Mn Ni S P Cr Ti Cu
0.9 - 1max   0.8max   0.8max   0.6max   0.025max   0.0317 - 19max   0.2max   0.3


Temperature of critical points for grade   95KH18   ( 95Х18 ).
Ac1 = 830 ,      Ac3(Acm) = 1100 ,       Ar3(Arcm) = 810


Mechanical properties under Т=20oС for grade   95KH18   ( 95Х18 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar     770 420 15 30 Annealing 885 - 920oC, 1 - 2h,


    Brinell hardness for     95KH18   ( 95Х18 )   (annealing) ,     Bar GOST 5949-75 HB 10 -1 = 269   MPa


Physical properties for grade   95KH18   ( 95Х18 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.04   24 7750    
100   11.8   7730 483  
200   12.3        
300   12.7        
400   13.1        
500   13.4        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     95KH18   ( 95Х18 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEuropeanPolandCzechia
-DIN,WNrJIS AFNOREN PNCSN
440B
440C
440FSe
A756
1.4125
X102CrMo17
X105CrMo17
SUS440C
X105CrMo17
Z100CD17
X102CrMo17
H18
17042

Types of delivery of grade   95KH18   ( 95Х18 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  95KH18   ( 95Х18 ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru