Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Stainless steel

Characteristics for grade     10KH17N13M2T   ( 10Х17Н13М2Т )

      Grade :   10KH17N13M2T   ( 10Х17Н13М2Т ) (   Х17Н13М2Т     ЭИ448   )
      Classification :   Corrosion-resistant steel for general purposes
      Equivalent grades:   Go here
Grade   10KH17N13M2T   ( 10Х17Н13М2Т ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 376-298-00 ,     info [a] auremo.org



Chemical composition in % for grade   10KH17N13M2T   ( 10Х17Н13М2Т )
C Si Mn Ni S P Cr Mo Cu -
max   0.1max   0.8max   212 - 14max   0.02max   0.03516 - 182 - 3max   0.3 (5 С - 0.7) Ti, остальное Fe


Mechanical properties under Т=20oС for grade   10KH17N13M2T   ( 10Х17Н13М2Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     529   35    
Pipe hot strain, GOST 9940-81     529   35    
Bar, GOST 5949-75 Ø 60   510 215 40 55 Guenching 1050 - 1100oC,Cooling air,
Wire, GOST 18143-72     540-830  20-25   
Forging, GOST 25054-81 to 1000   510 196 30-3845-50 Guenching 1050 - 1100oC, water,
Sheet trick, GOST 7350-77     530 235 37   Guenching 1030 - 1080oC,Cooling air,
Sheet thin, GOST 5582-75     530 225 38   Guenching 1050 - 1080oC,Cooling air,
Sheet thin, GOST 4986-79     530   20-40  Guenching 1050 - 1080oC, air,


    Brinell hardness for     10KH17N13M2T   ( 10Х17Н13М2Т )   ,     Forging GOST 25054-81 HB 10 -1 = 200   MPa


Technological properties for grade   10KH17N13M2T   ( 10Х17Н13М2Т )
  Weldability: without limitations.


Physical properties for grade   10KH17N13M2T   ( 10Х17Н13М2Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.06     7950    
100   15.7        
200 1.86 16.1        
300 1.77 16.7        
400 1.77 17.2        
500 1.67 17.6        
600 1.57 17.9        
700 1.47 18.2        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     10KH17N13M2T   ( 10Х17Н13М2Т )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenPolandCzechiaAustria
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSPNCSNONORM
316H
316Ti
318
S31635
1.4571
1.4583
X10CrNiMoNb18-12
X10CrNiMoTi18-10
X10CrNiMoTi18-12
X6CrNiMoTi17-12-2
SUS316Ti
Z6CNDNB17-12B
Z6CNDT17-12
Z6CNDT17-13
Z6NDT17-12
320S17
320S18
320S31
321S12
1.4571
X6CrNiMoTi17-12-2
X6CrNiMoTi17-12
F.3535
X6CrNiMoTi17-12-2
OCr18Ni12Mo2Ti
2350
2353
H17N13M2T
H18N10MT
17348
X6CrNiMoi17-17-122S

Types of delivery of grade   10KH17N13M2T   ( 10Х17Н13М2Т )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
B73 - Steel Alloy Wire
B76 - Metal nets


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  10KH17N13M2T   ( 10Х17Н13М2Т ) - Corrosion-resistant steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru