Characteristics for grade     VPr2   ( ВПр2 )



      Grade :   VPr2   ( ВПр2 ) (   ВПр-2   )
      Classification :   Copper-zinc solders
      Equivalent grades:     Is absent



Chemical composition in % for grade   VPr2   ( ВПр2 )
Fe Si Mn Ni CuLi Impurity -
0.6 - 1.20.1 - 0.522 - 265 - 665.55 - 71.650.15 - 0.25 all 0.5 Cu - basis
Comment: Zn is a basis; the percentage of Zn is given approximately.




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  VPr2   ( ВПр2 ) - Copper-zinc solders: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru