Characteristics for grade     13Kh16N3B   ( 13Х16Н3Б )



      Grade :     13Kh16N3B   ( 13Х16Н3Б )
      Classification :   Corrosion-resistant high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   13Kh16N3B   ( 13Х16Н3Б )
C Si Mn Ni S P Cr Nb Cu
0.1 - 0.150.2 - 0.70.4 - 0.82.2 - 2.8max   0.025max   0.02515.5 - 170.07 - 0.15max   0.3


Mechanical properties under Т=20oС for grade   13Kh16N3B   ( 13Х16Н3Б )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging to 200   590 440 15 35390 


    Brinell hardness for     13Kh16N3B   ( 13Х16Н3Б )   ,     Forging HB = 207 - 285   MPa




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  13Kh16N3B   ( 13Х16Н3Б ) - Corrosion-resistant high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru