Characteristics for grade     ZhS3DK   ( ЖС3ДК )

      Grade :   ZhS3DK   ( ЖС3ДК ) (   ЖС3ДК-ВИ   )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent
Grade   ZhS3DK   ( ЖС3ДК ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   ZhS3DK   ( ЖС3ДК )
Fe C Si Mn Ni S P Cr Ce Mo W Co TiAl B -
max   20.06 - 0.11max   0.4max   0.457.5 - 65.3max   0.01max   0.01511 - 12.5max   0.023.8 - 4.53.8 - 4.58 - 102.5 - 3.24 - 4.8max   0.02 Ni - basis
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   ZhS3DK   ( ЖС3ДК )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Blank     930   7  290 
Blank     880   5    


Material long term strength     ZhS3DK   ( ЖС3ДК )
OCT 1 90126-85
Test temperature   850 ° С
Acting stress   340   MPa
Time to fracture, hours   50

Types of delivery of grade   ZhS3DK   ( ЖС3ДК )
В32 - Graded and shaped rolling
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  ZhS3DK   ( ЖС3ДК ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru