Characteristics for grade     VZhL14N   ( ВЖЛ14Н )

      Grade :   VZhL14N   ( ВЖЛ14Н ) (   ВЖЛ14Н-ВИ   )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VZhL14N   ( ВЖЛ14Н )
Fe C Si Mn Ni S P Cr Ce Mo Nb TiAl B -
8 - 100.03 - 0.08max   0.4max   0.456.8 - 62.5max   0.015max   0.01518 - 20max   0.0254 - 51.8 - 2.82.5 - 2.91.2 - 1.5max   0.005 Ni - basis
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   VZhL14N   ( ВЖЛ14Н )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Blank     830   9 10390 


Material long term strength     VZhL14N   ( ВЖЛ14Н )
OCT 1 90126-85
Test temperature   600 ° С
Acting stress   590   MPa
Time to fracture, hours   100


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  VZhL14N   ( ВЖЛ14Н ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru