Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  

    YOU HERE:   Steel and Alloy   ->   High-temperature or heat-resistant steel and alloy

Characteristics for grade     VZhL18   ( ВЖЛ18 )

      Grade :   VZhL18   ( ВЖЛ18 ) (   ВЖЛ18-ВИ   )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VZhL18   ( ВЖЛ18 )
Fe C Si Mn Ni S P Cr Ce Mo W Co Nb TiAl Zr B PbBi -
max   10.1 - 0.15max   0.4max   0.455.1 - 64.1max   0.015max   0.01517 - 18max   0.024.5 - 62.5 - 44 - 61.2 - 1.82.2 - 33.4 - 4max   0.02max   0.06max   0.001max   0.0005 Ni - basis
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   VZhL18   ( ВЖЛ18 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Blank     880   2 2  


Material long term strength     VZhL18   ( ВЖЛ18 )
OCT 1 90126-85
Test temperature   900 ° С
Acting stress   240   MPa
Time to fracture, hours   40


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  VZhL18   ( ВЖЛ18 ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru