Characteristics for grade     VKh9L   ( ВХ9Л )

      Grade :   VKh9L   ( ВХ9Л ) (   ВХ9Л-ВИ   )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent
Grade   VKh9L   ( ВХ9Л ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   VKh9L   ( ВХ9Л )
Fe C Si Mn Ni S P Cr Mo W Co Nb TiAl B Ca Y -
max   60.02 - 0.1max   0.4max   0.544.1 - 54.8max   0.01max   0.01530 - 352.9 - 3.54.7 - 5.30.2 - 0.80.7 - 1.30.7 - 1.31 - 1.6max   0.005max   0.02max   0.04 Ni - basis
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   VKh9L   ( ВХ9Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Blank     780   5    


Material long term strength     VKh9L   ( ВХ9Л )
OCT 1 90126-85
Test temperature   800 ° С
Acting stress   180   MPa
Time to fracture, hours   100

Types of delivery of grade   VKh9L   ( ВХ9Л )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  VKh9L   ( ВХ9Л ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru