Characteristics for grade     VZhL1   ( ВЖЛ1 )

      Grade :   VZhL1   ( ВЖЛ1 ) (   ВЖЛ1-ВИ   )
      Classification :   High-temperature casting alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   VZhL1   ( ВЖЛ1 )
Fe C Si Mn Ni S P Cr Mo W TiAl B -
6 - 7.50.1 - 0.171.2 - 2max   0.359.5 - 66.1max   0.02max   0.0215 - 173.5 - 52 - 2.52 - 32 - 2.80.09 - 0.13 Ni - basis
Comment: Ni is a basis; the percentage of Ni is given approximately.


Mechanical properties under Т=20oС for grade   VZhL1   ( ВЖЛ1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Blank     670        


    Brinell hardness for     VZhL1   ( ВЖЛ1 )   ,       HB = 300 - 360   MPa


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

  VZhL1   ( ВЖЛ1 ) - High-temperature casting alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru