Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     12KH18N10T   ( 12Х18Н10Т )

      Grade :   12KH18N10T   ( 12Х18Н10Т ) (   Х18Н10Т   )
      Substitute:   08Х18Г8Н2Т, 10Х14Г14Н4Т, 12Х17Г9АН4, 08Х22Н6Т, 08Х17Т, 15Х25Т, 12Х18Н9Т
      Classification :   Сryogenic structural steel
      Equivalent grades:   Go here
Grade   12KH18N10T   ( 12Х18Н10Т ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   12KH18N10T   ( 12Х18Н10Т )
C Si Mn Ni S P Cr Cu -
max   0.12max   0.8max   29 - 11max   0.02max   0.03517 - 19max   0.3 (5 С - 0.8) Ti, остальное Fe


Mechanical properties under Т=20oС for grade   12KH18N10T   ( 12Х18Н10Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     549   35    
Pipe hot strain, GOST 9940-81     529   40    
Bar, GOST 5949-75 to Ø 60   510 196 40 55 Guenching 1020 - 1100oC,Cooling air,
Wire, GOST 18143-72     540-830  20-25   
Forging, GOST 25054-81 to 1000   510 196 35-3840-52 Guenching 1050 - 1100oC, water,
Sheet trick, GOST 7350-77     530 235 38   Guenching 1000 - 1080oC,Cooling water,
Sheet thin, GOST 5582-75     530 205 40   Guenching 1050 - 1080oC,Cooling water,
Sheet thin cold-worked , GOST 5582-75     880-1080  10    
Sheet thin, GOST 5582-75     740   25    


    Brinell hardness for     12KH18N10T   ( 12Х18Н10Т )   ,     Forging GOST 25054-81 HB 10 -1 = 179   MPa


Technological properties for grade   12KH18N10T   ( 12Х18Н10Т )
  Weldability: without limitations.
 Flakes : not predisposed


Physical properties for grade   12KH18N10T   ( 12Х18Н10Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.98   15 7920   725
100 1.94 16.6 16   462 792
200 1.89 17 18   496 861
300 1.81 17.2 19   517 920
400 1.74 17.5 21   538 976
500 1.66 17.9 23   550 1028
600 1.57 18.2 25   563 1075
700 1.47 18.6 27   575 1115
800   18.9 26   596  
900   19.3        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     12KH18N10T   ( 12Х18Н10Т )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaAustraliaSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSBDSMSZPNSTASCSNONORMASKS
321
321H
S32100
S32109
1.4541
1.4878
X10CrNiTi18-10
X12CrNiTi18-9
X6CrNiTi18-10
SUS321
Z10CNT18-10
Z10CNT18-11
Z6CNT18-10
Z6CNT18-12
321S31
321S51
321S59
LW18
LW24
X6CrNiTi18-10
1.4541
1.4878
X10CrNiTi18-10
X6CrNiTi18-10KT
X6CrNiTi18-11
X6CrNiTi18-11KG
X6CrNiTi18-11KT
F.3523
X6CrNiTi18-10
0Cr18Ni10Ti
0Cr18Ni11Ti
0Cr18Ni9Ti
1Cr18Ni11Ti
H0Cr20Ni10Ti
2337
0Ch18N10T
Ch18N12T
Ch18N9T
X6CrNiTi18-10
H5Ti
KO36Ti
KO37Ti
X6CrNiTi18-10
0H18N10T
1H18N10T
1H18N12T
1H18N9T
10TiNiCr180
12TiNiCr180
17246
17247
17248
X6CrNiTi18-10KKW
X6CrNiTi18-10S
321
STS321
STS321TKA
STSF321

Types of delivery of grade   12KH18N10T   ( 12Х18Н10Т )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
B73 - Steel Alloy Wire
B76 - Metal nets


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  12KH18N10T   ( 12Х18Н10Т ) - Сryogenic structural steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru