Grade : | 08Kh15N5D2TU ( 08Х15Н5Д2ТУ ) ( 08Х15Н5Д2ТУ-Ш ЭП410У ЭП410У-Ш 08Х15Н5Д2ТУ-ВД ЭП410У-ВД ) |
Classification : | Corrosion-resistant high-temperature steel |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | Ti | Cu |
max 0.08 | max 0.7 | max 1 | 4.8 - 5.8 | max 0.018 | max 0.02 | 13.5 - 14.8 | 0.03 - 0.15 | 1.75 - 2.5 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar | Ø 80 | 1080 | 785 | 10 | 55 | 1200 | Guenching 950oC,Cooling air, |
В22 - Graded and shaped rolling |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |