Chemical composition in % for grade   06KHN28MDT   ( 06ХН28МДТ )
Fe C Si Mn Ni S P Cr Mo Ti Cu
36.885 - 46.5max   0.06max   0.8max   0.826 - 29max   0.02max   0.03522 - 252.5 - 30.5 - 0.92.5 - 3.5


Mechanical properties under Т=20oС for grade   06KHN28MDT   ( 06ХН28МДТ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     490   30    
Forging, GOST 25054-81     510 216 30-3630-40  
Blank for pipe     540 245 35 50980Guenching 1050 - 1080oC, water,
Sheet trick, GOST 7350-77     540 215 35   Guenching 950 - 1080oC,Cooling water,
Sheet thin, GOST 5582-75     540   35   Guenching 1050 - 1080oC,Cooling water,
Sheet thin, GOST 4986-79     550   13-25  Guenching 930 - 1050oC,Cooling air,


    Brinell hardness for     06KHN28MDT   ( 06ХН28МДТ )   ,     Forging GOST 25054-81 HB 10 -1 = 200   MPa


Technological properties for grade   06KHN28MDT   ( 06ХН28МДТ )
  Weldability: without limitations.


Physical properties for grade   06KHN28MDT   ( 06ХН28МДТ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20     13 7960   750
100 1.91 10.9 13      
200 1.86 12.9 15      
300 1.79 13.6 17      
400 1.71 14.4        
500 1.61 14.9 22      
600 1.56 15.3 24      
700 1.51 16.8 25      
800 1.45 16.3 26      
900   16.8        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     06KHN28MDT   ( 06ХН28МДТ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFrance
-DIN,WNrJIS AFNOR
N08028
1.4563
SCS23
Z1NCDU31-27-03



Types of delivery of grade   06KHN28MDT   ( 06ХН28МДТ )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  06KHN28MDT   ( 06ХН28МДТ ) - Corrosion-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru