Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     07GFB   ( 07ГФБ )

      Grade :     07GFB   ( 07ГФБ )
      Classification :   Structural steel for welding construct
      Equivalent grades:     Is absent



Chemical composition in % for grade   07GFB   ( 07ГФБ )
C Si Mn Ni S P Cr Ce V N Nb TiAl Cu As Ca
0.06 - 0.090.2 - 0.40.8 - 1.2max   0.3max   0.035max   0.03max   0.3max   0.050.04 - 0.08max   0.0120.02 - 0.060.01 - 0.0350.02 - 0.05max   0.3max   0.08max   0.05


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  07GFB   ( 07ГФБ ) - Structural steel for welding construct: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru