Grade : | 14G2AF-1 ( 14Г2АФ-1 ) |
Classification : | Structural steel for welding construct |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | V | N | Cu | As |
0.12 - 0.18 | max 0.6 | max 1.6 | max 0.3 | max 0.035 | max 0.03 | max 0.4 | 0.07 - 0.12 | 0.015 - 0.025 | max 0.3 | max 0.08 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet | to 50 | 510 | 390 | 19 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |