Characteristics for grade     20KH23N13   ( 20Х23Н13 )

      Grade :   20KH23N13   ( 20Х23Н13 ) (   Х23Н13     ЭИ319   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here
Grade   20KH23N13   ( 20Х23Н13 ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   20KH23N13   ( 20Х23Н13 )
C Si Mn Ni S P Cr Ti Cu
max   0.2max   1max   212 - 15max   0.025max   0.03522 - 25max   0.2max   0.3


Mechanical properties under Т=20oС for grade   20KH23N13   ( 20Х23Н13 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 Ø 60   490 295 35 50 Guenching 1100 - 1150oC, air,
Sheet trick, GOST 7350-77     570   35   Guenching
Sheet thin, GOST 5582-75     540   35   Guenching 1100 - 1150oC,Cooling air,


Technological properties for grade   20KH23N13   ( 20Х23Н13 )
  Weldability: limited weldability.
Temper brittleness: predisposed


Physical properties for grade   20KH23N13   ( 20Х23Н13 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.07     7820    
100   14.9   7790 538  
200   15.7 17      
300   16.6 19      
400   17.1 21      
500   17.5 23      
600   17.8 24 7580    
700   18.2 27      
800     29 7480    
900     31      
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     20KH23N13   ( 20Х23Н13 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaPolandSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBPNKS
309
MT309
MT309S
S30900
S30908
X12CrNi23-13
X7CrNi23-14
X9CrNiSiNCe21-11-2
SUH309
SUS309
SUS309S
SUS309STB
Z15CN24-13
309S
309S16
309S24
X12CrNi23-13
1.4833
X12CrNi23-13
X16CrNi23-14
X12CrNi23-13
0Cr23Ni13
H23N13
STS309S

Types of delivery of grade   20KH23N13   ( 20Х23Н13 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  20KH23N13   ( 20Х23Н13 ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru