Characteristics for grade     10KH23N18   ( 10Х23Н18 )

      Grade :   10KH23N18   ( 10Х23Н18 ) (   0Х23Н18   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here



Chemical composition in % for grade   10KH23N18   ( 10Х23Н18 )
C Si Mn Ni S P Cr Ti Cu
max   0.1max   1max   217 - 20max   0.02max   0.03522 - 25max   0.2max   0.3


Mechanical properties under Т=20oС for grade   10KH23N18   ( 10Х23Н18 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe cooling strain, GOST 9941-81     529   35    
Pipe hot strain, GOST 9940-81     491   37    
Bar, GOST 5949-75 Ø 60   490 196 35 50 Guenching 1100 - 1150oC, air,
Forging, GOST 25054-81     490 196 30-3540-47  


    Brinell hardness for     10KH23N18   ( 10Х23Н18 )   (quenching) ,       GOST 25054-81 HB 10 -1 = 179   MPa


Technological properties for grade   10KH23N18   ( 10Х23Н18 )
Temper brittleness: predisposed


Physical properties for grade   10KH23N18   ( 10Х23Н18 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7950    


Equivalent steels for grade     10KH23N18   ( 10Х23Н18 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenAustralia
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSAS
310S
S31000
S31008
S31009
1.4842
1.4845
X10CrNiSiN21-11
X12CrNi25-20
X12CrNi25-21
X8CrNi25-21
X9CrNiSiNCe21-11-2
SUH310
SUS310S
Z12CN25-20
Z12CN26-21
Z8CN25-20
310S16
310S24
310S94
X8CrNi25-21
1.4842
X8CrNi25-21
X6CrNi25-20
F.331
X8CrNi25-21
0Cr25Ni20
2361
310S


Assortment for grade   10KH23N18   ( 10Х23Н18 )
B03 - Metal forming treatment. Forgings
  GOST   25054 - 81 Forgins of corrosion-resisting steels and alloys
В22 - Graded and shaped rolling
  GOST   1133 - 71 Forged round and square steel
  GOST   2590 - 2006 Steel hot-rolled round bars
  GOST   2591 - 2006 Steel hot-rolled square bars
  GOST   2879 - 2006 Hot-rolled hexagonal steel
B23 - Sheets and Strips
  GOST   103 - 2006 Hot-rolled steel strip
В32 - Graded and shaped rolling
  GOST   8559 - 75 Calibrated square steel
  GOST   5949 - 75 Sorted and gauged corrosion-resistant, heat-resistant and high-temperature steel
  GOST   7417 - 75 Calibrated round steel
B33 - Sheets and Strips
  GOST   4405 - 75 Hot-rolled and wrought tool steel strips
В62 - Steel pipes and connecting parts to them
  GOST   9940 - 81 Seamless hot deformed tubes made of corrosion resistant steel
  GOST   9941 - 81 Seamles cold and warm deformed tubes made of corrosion resistant steel


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  10KH23N18   ( 10Х23Н18 ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru