Characteristics for grade     20KH25N20S2   ( 20Х25Н20С2 )

      Grade :   20KH25N20S2   ( 20Х25Н20С2 ) (   Х25Н20С2     ЭИ283   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here
Grade   20KH25N20S2   ( 20Х25Н20С2 ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   20KH25N20S2   ( 20Х25Н20С2 )
Fe C Si Mn Ni S P Cr Mo W V Ti Cu
46.045 - 56max   0.22 - 3max   1.518 - 21max   0.02max   0.03524 - 27max   0.3max   0.2max   0.2max   0.2max   0.3


Mechanical properties under Т=20oС for grade   20KH25N20S2   ( 20Х25Н20С2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 5949-75 Ø 60   590 295 35 50 Guenching 1100 - 1150oC, air,
Sheet thin, GOST 5582-75     490   35   Guenching 1050 - 1100oC,Cooling water,


Technological properties for grade   20KH25N20S2   ( 20Х25Н20С2 )
Temper brittleness: predisposed


Physical properties for grade   20KH25N20S2   ( 20Х25Н20С2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7720    
100   16.1 15 7680    
200            
300            
400            
500     22      
600   17.8 24      
700   17.8 25      
800   18.1 27 7440    
900   18.5 29 7390    
1000   18.8        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     20KH25N20S2   ( 20Х25Н20С2 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenPolandCzechia
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSPNCSN
310
314
S31400
1.4841
CrNi25-20
X15CrNiSi25-20
X15CrNiSi25-21
SUH310
SUS18
SUSY310
Z12CN25.20
Z15CNS25-20
310S24
314S25
1.4841
X15CrNiSi25-20
X16CrNiSi25-20
X25CN25-20
F.3310
X15CrNiSi25-20
2Cr25Ni20
2376
H25N20S2
17255

Types of delivery of grade   20KH25N20S2   ( 20Х25Н20С2 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  20KH25N20S2   ( 20Х25Н20С2 ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru