Characteristics for grade     15GS   ( 15ГС )

      Grade :   15GS   ( 15ГС ) (   15ГС-Ш   )
      Classification :   Structural steel for welding construct
      Equivalent grades:     Is absent



Chemical composition in % for grade   15GS   ( 15ГС )
C Si Mn Ni S P Cr Mo Cu
0.12 - 0.180.7 - 10.9 - 1.3max   0.3max   0.025max   0.035max   0.3max   0.15max   0.3


Mechanical properties under Т=20oС for grade   15GS   ( 15ГС )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe   longitudinal 500   18 45 Normalizing 900 - 930oC, air,
Pipe   dihedral 500   16 40 Normalizing 900 - 930oC, air,


Technological properties for grade   15GS   ( 15ГС )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  15GS   ( 15ГС ) - Structural steel for welding construct: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru