YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     St3kp   ( Ст3кп )

      Grade :     St3kp   ( Ст3кп )
      Classification :   Normal quality structural carbon steel
      Equivalent grades:   Go here



Chemical composition in % for grade   St3kp   ( Ст3кп )
C Si Mn Ni S P Cr N Cu As
0.14 - 0.22max   0.050.3 - 0.6max   0.3max   0.05max   0.04max   0.3max   0.008max   0.3max   0.08


Mechanical properties under Т=20oС for grade   St3kp   ( Ст3кп )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 8696-74     363 235 23    
Pipe, GOST 10705-80     372 225 22    
Rolled stock, GOST 535-2005     360-460195-23524-27   
Sheet trick, GOST 14637-89     360-460195-23524-27   
Rebar, GOST 5781-82     373 235 25    
Wire rods , GOST 30136-95     490-540    60  


    Brinell hardness for     St3kp   ( Ст3кп )   ,       HB 10 -1 = 131   MPa


Technological properties for grade   St3kp   ( Ст3кп )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed


Physical properties for grade   St3kp   ( Ст3кп )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7850    


Equivalent steels for grade     St3kp   ( Ст3кп )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandCanadaEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaInter
-DIN,WNrJIS AFNORBSHGEN UNINBNUNEGBSSBDSMSZPNSTASCSNONORMISO
A283(A)
A284Gr.D
A570(33)
A570(36)
A573Gr.58
A611Gr.C
K01804
K02001
K02301
K02502
K02601
K02701
K02702
1.0036
1.0036
1.0116
Fe360B
Fe360D1
RSt37-2
S235J2G3
S235JRG1
USt37-2
USt37-2G
SS400
STKM12A
4360-40D
E24-3
E24-4
S235J0
S235J2G3
S235J2G4
S235JRG1
1449-37/23CR
235JRG1
4360-40B
4449-250
Fe360B
Fe360D1FF
HFS4
HFW4
S235J2G3
230G
1.0036
Fe37-3FN
Fe37-3FU
Fe37B1FN
Fe37B1FU
Fe37B3FN
Fe37B3FU
S235J2G3
S235JRG1
Fe360B
Fe360BFU
Fe360C
Fe360CFN
Fe360D
Fe360DFF
Fe37-2
S235J0
S235J2G3
S235J2G4
S235JRG1
FE360B
FED1FF
AE235B
AE235D
Fe360B
Fe360D1FF
S235J2G3
S235JRG1
A3
Q235
Q235A
Q235A-F
Q235A-Z
Q235B
Q235B-Z
1311
1312
1313
BSt3kp
BSt3ps
Ew-08AA
S235J2G3
S235JRG1
WSt3kp
A1
B38.24
B38.24B
Fe235B/FU
S235J2G3
S235JRG1
SS400
St3SX
St3SY
St3W
OB37
OL37.1
10216
11373
11378
St37F
E235-A
Fe360-A

Types of delivery of grade   St3kp   ( Ст3кп )
B03 - Metal forming treatment. Forgings
В20 - Classification, nomenclature and general norms
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
B34 - Ribbons
B42 - Rails: Pads, Pads, Crutches
В62 - Steel pipes and connecting parts to them
B76 - Metal nets


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  St3kp   ( Ст3кп ) - Normal quality structural carbon steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru