Characteristics for grade     15GF   ( 15ГФ )

      Grade :     15GF   ( 15ГФ )
      Classification :   Structural steel for welding construct
      Equivalent grades:   Go here



Chemical composition in % for grade   15GF   ( 15ГФ )
C Si Mn Ni S P Cr V N Cu As
0.12 - 0.180.17 - 0.370.9 - 1.2max   0.3max   0.035max   0.03max   0.30.05 - 0.12max   0.012max   0.3max   0.08


Mechanical properties under Т=20oС for grade   15GF   ( 15ГФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet, GOST 19282-73     510 375 21    
Bars to 140   480 345 21    


Technological properties for grade   15GF   ( 15ГФ )
  Weldability: without limitations.
 Flakes : not predisposed
Temper brittleness: not predisposed


Equivalent steels for grade     15GF   ( 15ГФ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainSwedenBulgariaHungaryPolandRomaniaFinland
-DIN,WNrJIS AFNORBSEN UNIUNESSBDSMSZPNSTASSFS
A588
A633Gr.C
A852
K01600
K02700
K02701
K02803
K11430
1.0562
P355N
StE355
SM490A
SM490B
SM490C
SM490YA
SM490YB
STK490
E355R/FP
FeE355KGN
P355N
S355M
S355ML
S355N
S355NL
P355N
1.0562
FeE355A
P355N
S355N
FeE355KG
FeE355KKW
P355N
AE355DD
AE355KG
P355N
2106
10G2SBSBB
10G2SFTSFT
52D
18G2A
OCS355.5a
RAEX355N
RAEX384P

Types of delivery of grade   15GF   ( 15ГФ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  15GF   ( 15ГФ ) - Structural steel for welding construct: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru