Characteristics for grade     16D   ( 16Д )

      Grade :   16D   ( 16Д ) (   16Д-Ш   )
      Classification :   Structural steel for welding construct
      Equivalent grades:   Go here



Chemical composition in % for grade   16D   ( 16Д )
C Si Mn Ni S P Cr N Cu As
0.1 - 0.180.12 - 0.250.4 - 0.7max   0.3max   0.04max   0.035max   0.3max   0.0080.2 - 0.35max   0.08


Mechanical properties under Т=20oС for grade   16D   ( 16Д )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rolled stock, GOST 6713-91     375-510215-23526  340-390 


Equivalent steels for grade     16D   ( 16Д )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandCanadaEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaFinlandAustria
-DIN,WNrJIS AFNORBSHGEN UNINBNUNEGBSSBDSMSZPNSTASCSNSFSONORM
A284Gr.D
A570Gr.33,36
A573Gr.58
A611(A)
A611Gr.C
K01804
K02001
K02301
K02502
K02601
K02701
K02702
1.0028
1.0036
1.0116
Fe360B
Fe360D1
S235J2G3
S235JRG1
St34-2
St37-3
St37-3G
USt37-2G
SS330
A34-2
E24-3
E24-4
S235J0
S235J2G3
S235J2G4
S235JRG1
1449-37/23CR
37/23HR
4360-40D
CEW2BK
Fe360B
Fe360D1FF
HFS4
HFW4
S235J2G3
S235JRG1
230G
1.0036
Fe37-3FN
Fe37-3FU
Fe37B1
Fe37B1FN
Fe37B1FU
Fe37B3FN
Fe37B3FU
S235J2G3
S235JRG1
Fe330
Fe360B
Fe360BFU
Fe360C
Fe360CFN
Fe360D
Fe360DFF
Fe37-2
S235J0
S235J2G3
S235J2G4
S235JRG1
FE360B
FED1FF
AE235B
AE235D
Fe360D1FF
S235J2G3
S235JR
S235JRG1
A3
Q235A
Q235A-F
Q235A-Z
Q235B
Q235B-F
Q235B-Z
1311
1312
1313
BSt3kp
Ew-08AA
S235J2G3
S235JRG1
WSt3kp
Fe235B/FU
Fe235D
S235J2G3
S235JRG1
St3SX
St3W
OL37.4
11343
11373
11378
RACOLD215S
St34RG
St37TK

Types of delivery of grade   16D   ( 16Д )
В22 - Graded and shaped rolling
B23 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  16D   ( 16Д ) - Structural steel for welding construct: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru