Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Cast iron

Characteristics for grade     SCH15   ( СЧ15 )

      Grade :     SCH15   ( СЧ15 )
      Classification :   Grey cast iron
      Equivalent grades:   Go here



Chemical composition in % for grade   SCH15   ( СЧ15 )
C Si Mn S P
3.5 - 3.72 - 2.40.5 - 0.8max   0.15max   0.2


Mechanical properties under Т=20oС for grade   SCH15   ( СЧ15 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 1412-85     150        


    Brinell hardness for     SCH15   ( СЧ15 )   ,       GOST 1412-85 HB 10 -1 = 130 - 241   MPa


Technological properties of the material   SCH15   ( СЧ15 ) .
        Linear shrinkage : 1.1   %


Physical properties for grade   SCH15   ( СЧ15 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.9   59 7000    
100   9     460  


Equivalent steels for grade     SCH15   ( СЧ15 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaAustriaAustraliaInterIndiaHollandTaiwanLuxembourgCOPANT
-DIN,WNrJIS AFNORBSEN UNINBNUNEGBSSBDSMSZPNSTASCSNONORMASISOISNEN--COPANT
A48-25B
C1.25B
No.25
GG15
FC15
FC150
FGL150
Ft15D
150
Gr.150
EN-GJL-150
EN-JL1020
G15
FGG15
FG15
HT150
0115-00
O115
Vch15
OV15
Z115
ZI150
FC150
422415
GG15
GG150
T150
150
FG150
GG15
FC150
FGG15
FG150

Types of delivery of grade   SCH15   ( СЧ15 )
B11 - Cast Iron
В61 - Pipes of ferrous metals and alloys cast and connecting parts to them
В81 - Castings of cast iron (gray and malleable cast iron)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  SCH15   ( СЧ15 ) - Grey cast iron: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru