Characteristics for grade     CHNMSH   ( ЧНМШ )



      Grade :     CHNMSH   ( ЧНМШ )
      Classification :   Low alloy cast iron
      Equivalent grades:     Is absent



Chemical composition in % for grade   CHNMSH   ( ЧНМШ )
C Si Mn Ni S P Cr Mo
2.8 - 3.81.7 - 3.20.8 - 1.20.8 - 1.5max   0.03max   0.1max   0.10.3 - 0.7


Mechanical properties under Т=20oС for grade   CHNMSH   ( ЧНМШ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 7769-82     490   2    


    Brinell hardness for     CHNMSH   ( ЧНМШ )   ,       GOST 7769-82 HB 10 -1 = 183 - 286   MPa



Types of delivery of grade   CHNMSH   ( ЧНМШ )
В81 - Castings of cast iron (gray and malleable cast iron)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  CHNMSH   ( ЧНМШ ) - Low alloy cast iron: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru