Characteristics for grade     9KH5VF   ( 9Х5ВФ )

      Grade :     9KH5VF   ( 9Х5ВФ )
      Classification :   Alloy tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   9KH5VF   ( 9Х5ВФ )
C Si Mn Ni S P Cr W V Cu
0.85 - 10.1 - 0.40.15 - 0.45max   0.4max   0.03max   0.034.5 - 5.50.8 - 1.20.15 - 0.3max   0.3


Temperature of critical points for grade   9KH5VF   ( 9Х5ВФ ).
Ac1 = 815 ,      Ac3(Acm) = 830 ,       Ar1 = 755 ,       Mn = 240


    Brinell hardness for     9KH5VF   ( 9Х5ВФ )   (annealing) ,       GOST 5950-2000 HB 10 -1 = 241   MPa


Equivalent steels for grade     9KH5VF   ( 9Х5ВФ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenPolandCzechiaAustria
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSPNCSNONORM
A2
T30102
X100CrMoV5-1
SKD12
X100CrMoV5
Z100CDV5
BA2
1.2363
X100CrMoV5-1
X100CrMoV51KU
X100CrMoV5
Cr5Mo1V
2260
NCLV
19571
BOHLERK305
K305

Types of delivery of grade   9KH5VF   ( 9Х5ВФ )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  9KH5VF   ( 9Х5ВФ ) - Alloy tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru