Characteristics for grade     6KH3MFS   ( 6Х3МФС )



      Grade :   6KH3MFS   ( 6Х3МФС ) (   ЭП788   )
      Classification :   Alloy tool steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   6KH3MFS   ( 6Х3МФС )
C Si Mn Ni S P Cr Mo V Cu
0.55 - 0.620.35 - 0.650.2 - 0.6max   0.4max   0.03max   0.032.6 - 3.30.2 - 0.50.3 - 0.6max   0.3


Temperature of critical points for grade   6KH3MFS   ( 6Х3МФС ).
Ac1 = 760 - 790 ,      Ac3(Acm) = 950 - 975 ,       Mn = 210 - 220


    Brinell hardness for     6KH3MFS   ( 6Х3МФС )   (annealing) ,       GOST 5950-2000 HB 10 -1 = 241   MPa



Types of delivery of grade   6KH3MFS   ( 6Х3МФС )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  6KH3MFS   ( 6Х3МФС ) - Alloy tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru