Characteristics for grade     15KH13L   ( 15Х13Л )

      Grade :     15KH13L   ( 15Х13Л )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:   Go here



Chemical composition in % for grade   15KH13L   ( 15Х13Л )
C Si Mn S P Cr
max   0.150.2 - 0.80.3 - 0.8max   0.025max   0.0312 - 14


Mechanical properties under Т=20oС for grade   15KH13L   ( 15Х13Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     540 392 16 45491Annealing 950oC,Guenching 1050oC,Cooling Drawing 750oC,Cooling air,


Heat treatment of the material   15KH13L   ( 15Х13Л )
Annealing 940 - 960 ° C, Hardening 1040 - 1060 ° C, Oil or air cooling; Tempering 740 - 760 ° C , Air cooling;


Equivalent steels for grade     15KH13L   ( 15Х13Л )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaFinlandAustriaAustraliaSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSBDSMSZPNSTASCSNSFSONORMASKS
410
Gr.CA40
J91150
J91171
J91201
S41000
S41001
1.4006
GX12Cr13
X10Cr13
X12Cr13
SCS1
SUS410
Z10C13
Z12C13
Z12C13-M
410C21
410S21
ANC1A
X12Cr13
1.4006
X10Cr13
X12Cr13
X12Cr13KD
GX12Cr13
X10Cr13
X12Cr13
X12Cr9KG
F.3401
X10Cr13
1Cr12
1Cr13
ZG15Cr13
ZG1Cr13
2302
1Ch13
1Ch13L
X12Cr13
AoX12Cr13
KO2
X12Cr13
1H13
LOH13
10Cr130
12C130
T15Cr130
17021
422905
G-X12Cr13
BOHLERN100
410
STS410
STS410TKA
STSF410-A
STSF410-B
STSF410-C
STSF410-D

Types of delivery of grade   15KH13L   ( 15Х13Л )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  15KH13L   ( 15Х13Л ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru