Characteristics for grade     18KHG   ( 18ХГ )

      Grade :     18KHG   ( 18ХГ )
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   18KHG   ( 18ХГ )
C Si Mn Ni S P Cr Cu
0.15 - 0.210.17 - 0.370.9 - 1.2max   0.3max   0.035max   0.0350.9 - 1.2max   0.3


Temperature of critical points for grade   18KHG   ( 18ХГ ).
Ac1 = 765 ,      Ac3(Acm) = 840


Mechanical properties under Т=20oС for grade   18KHG   ( 18ХГ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 15   880 735 10 40 Guenching 880oC, oil, Drawing 200oC, air,


    Brinell hardness for     18KHG   ( 18ХГ )   (annealing) ,       GOST 4543-71 HB 10 -1 = 187   MPa


Technological properties for grade   18KHG   ( 18ХГ )
 Flakes : predisposed
Temper brittleness: predisposed


Equivalent steels for grade     18KHG   ( 18ХГ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyBelgiumSpainChinaSwedenBulgariaHungaryPolandRomaniaCzechiaFinlandAustraliaSouth Korea
-DIN,WNrJIS AFNORBSEN UNINBNUNEGBSSBDSMSZPNSTASCSNSFSASKS
5115
5120
G51150
G51200
H51200
1.7131
1.7147
16MnCr5
16MnCrS5
20MnCr5
20MnCrS5
SMnC420
SMnC420H
16MC4
16MC5
16MnCr5RR
20MC5
16MnCr5
20MnCr5
527M17
527M20
590H17
590M17
1.7131
1.7147
16MnCr5
16MnCr5KD
20MnCr5
20MnCrB5
16MnCr5
20MnCr5
16MnCr5
16MnCr5
20MnCr5
F.1516
15CrMn
20CrMn
2127
2173
16ChG
18ChG
BC3
BC3Z
15HG
16HG
18HGT
20HG
17MnCr10
18MnCr10q
18MnCr11
20MnCr12
14220
14221
14222
14223
20MnCr5
5120
5120H
SMnC420H

Types of delivery of grade   18KHG   ( 18ХГ )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  18KHG   ( 18ХГ ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru