Characteristics for grade     40KHMFА   ( 40ХМФА )

      Grade :     40KHMFА   ( 40ХМФА )
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   40KHMFА   ( 40ХМФА )
C Si Mn Ni S P Cr Mo V Cu
0.37 - 0.440.17 - 0.370.4 - 0.7max   0.3max   0.025max   0.0250.8 - 1.10.2 - 0.30.1 - 0.18max   0.3


Mechanical properties under Т=20oС for grade   40KHMFА   ( 40ХМФА )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 25   1030 930 13 50880Guenching 860oC, oil, Drawing 580oC, oil,


    Brinell hardness for     40KHMFА   ( 40ХМФА )   (annealing) ,       GOST 4543-71 HB 10 -1 = 269   MPa


Equivalent steels for grade     40KHMFА   ( 40ХМФА )
Warning! Indicated both exact and nearest equivalents.
BulgariaPoland
BDSPN
40ChMFA
40H2MF

Types of delivery of grade   40KHMFА   ( 40ХМФА )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  40KHMFА   ( 40ХМФА ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru