Characteristics for grade     20KHGNTR   ( 20ХГНТР )

      Grade :     20KHGNTR   ( 20ХГНТР )
      Classification :   Alloy structurall steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   20KHGNTR   ( 20ХГНТР )
C Si Mn Ni S P Cr Ti Cu B
0.18 - 0.240.17 - 0.370.8 - 1.10.4 - 0.7max   0.035max   0.0350.4 - 0.70.03 - 0.09max   0.30.001 - 0.005


Mechanical properties under Т=20oС for grade   20KHGNTR   ( 20ХГНТР )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 15   1180 980 9 50780Guenching 850oC, oil, Drawing 200oC, oil,


    Brinell hardness for     20KHGNTR   ( 20ХГНТР )   ,     Rolled stock GOST 4543-71 HB 10 -1 = -1   MPa


Technological properties for grade   20KHGNTR   ( 20ХГНТР )
 Flakes : not predisposed
Temper brittleness: predisposed

Types of delivery of grade   20KHGNTR   ( 20ХГНТР )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  20KHGNTR   ( 20ХГНТР ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru